Analysis of the causes of uneven color of woven bags The main reasons and solutions for uneven color of woven bags are as follows:
(1) Poor diffusion of the colorant, which often causes patterns to appear near the gate.
(2) Plastic woven bags or colorants have poor thermal stability. To stabilize the color of woven bags, the production conditions must be strictly fixed, especially the material temperature, material volume and production cycle.
(3) For crystalline plastic woven bags, try to make the cooling rate of each part of the woven bag consistent. For woven bags with large wall thicknesses, enterprises supplying waste woven bags can use colorants to mask the color difference. For woven bags with uniform wall thickness The material temperature and mold temperature must be fixed.
(4) The shape of the woven bag, the form of the gate, and the position of the woven bag have an impact on the filling of the plastic woven bag, causing some parts of the woven bag to produce color differences, which should be modified if necessary.
Analysis of the causes of color and gloss defects of woven bags Under normal circumstances, the gloss on the surface of injection-molded woven bags is mainly determined by the type of plastic woven bags, colorants and the finish of the mold surface.
But often due to some other reasons, the surface color and gloss defect of the woven bag, the surface dark color and other defects.

The reasons and solutions are as follows:
(1) Poor mold finish, rust marks on the surface of the cavity, and poor mold exhaust.
(2) The gating system of the mold is defective, the cold slug well should be enlarged, the runner, polished main runner, runner and gate should be enlarged.
(3) The material temperature and mold temperature are low, and local heating of the gate can be used if necessary.
(4) The processing pressure is too low, the speed is too slow, the injection time is insufficient, and the back pressure is insufficient, resulting in poor compactness and dark surface.
(5) Plastic woven bags must be fully plasticized, but to prevent material degradation, be stable when heated, and adequately cooled, especially thick-walled ones.
(6) Prevent cold materials from entering the woven bag, and use self-locking springs or lower the nozzle temperature when necessary.
(7) The waste woven bags used are too much powder, the plastic woven bags or colorants are of poor quality, mixed with water vapor or other impurities, and the lubricants used by the enterprises supplying the waste woven bags are of poor quality.
(8) The clamping force must be sufficient.